Using CA to glue the flap did fix the burn-through problem at the nozzle. However, further tests had blistering at the delay section at 5-7 seconds and burn through at 10+ seconds. We would never have a delay that long, but it does show a potential problem with external case heating.

In cutting open many of the casings, I noticed that the layers are not glued as well as the 18mm casings made at the same time. I suspect NEPT has problems with tubes that small.

We have refiitted to 18mm and will put the 10mm on hold until we have more resources (time, money) to continue trying to make them work.

Thanks to all for the suggestions!
__________________
Carl McLawhorn
NAR#4717 L2
semroc.com
Reply With Quote
 


Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump



All times are GMT -5. The time now is 10:54 AM.


Powered by: vBulletin Version 3.0.7
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Ye Olde Rocket Shoppe © 1998-2024